Material: | Black Polypropylene |
Method Used: | Etch |
Depth: | <.001 |
Laser Type: | 20 watt Q-Switch Fiber Laser |
Focal Length Lens: | 160mm |
Power: | 30 – 100% |
Frequency: | 20kHz |
Speed: | 26 – 60 inches per second |
Passes: | 1 |
Cycle Time: | 156 – 188ms |
Samples were processed using a 20 watt Q-switched fiber laser through a 160mm F-theta lens