Laser marking of the machined rubber/aluminum tube was accomplished using a 10 Watt Fiber Laser Marking System. The marking on the tube had a long cycle time of 8.91 seconds. The rubber was marked slower to produce a deeper mark. The parts were marked using a 10-watt Fiber Laser Marking System.