Material: aluminum Method Used: etch Depth: < 3mm Laser Type: 20 Watt Q-Switch Fiber Laser Focal Length Lens: 160mm Power: 100% Frequency: 20 kHz Speed: 10 inches per second Passes: 600 Cycle Time: 10 mins SamplesRead More…
Material: aluminum Method Used: etch Depth: < 3mm Laser Type: 20 Watt Q-Switch Fiber Laser Focal Length Lens: 160mm Power: 100% Frequency: 20 kHz Speed: 10 inches per second Passes: 600 Cycle Time: 10 mins SamplesRead More…
Material: Carbon Pieces – 2nd Trial Method Used: Etch Depth: <.002 Laser Type: 20 watt Q-Switch Fiber Laser Focal Length Lens: 160mm Power: 100% Frequency: 20kHz Speed: 10 inches per second Passes: 9 Cycle Time: 57Read More…
Material: Titanium Method Used: Annealing Depth: Surface Laser Type: Pulsed Fiber Focal Length Lens: 160mm Power: 95% Frequency: 30 kHz Speed: 1″ per sec Passes: 12 Cycle Time: 26.52 seconds The samples were processed using theRead More…
Material: pills Power: 20% Method Used: Etch Frequency: 30KHz Depth: <.001 Speed: 10 inches per second Laser Type: 20 Watt Q-Switch Fiber Laser Passes: 1 Focal Length Lens: 160mm Cycle Time: 1.328sec Samples were processed usingRead More…
Material: stainless steel Power: 98% Method Used: annealed Frequency: 35 kHz Depth: <.001 Speed: 5 inches per second Laser Type: 20 Watt Q-Switch Fiber Laser Read More…
Sample was processed using a 20 watt Q-switched fiber laser through a 160mm F-theta lens.
Material: Stainless steel and gold Power: 95% Method Used: etch Frequency: 20 kHz Depth: <.001 Speed: 10 inches per second Laser Type: 20 Watt Q-Switch FiberRead More…
Sample was processed using a 20 watt Q-switched fiber laser through a 160mm F-theta lens.
Sample was processed using a 20 watt Q-switched fiber laser through a 160mm F-theta lens.
Material: aluminum Power: 50% Method Used: etch Frequency: 35kHz Depth: <.002 Speed: 25 inches per second Laser Type: 20 Watt Q-Switch Fiber Laser Passes: 1 Focal Length Lens: 160mm Cycle Time: 15.6 seconds Sample was processedRead More…